HUMISEAL UV23
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Fast 30-Second UV Handling
- Dual Secondary Cure Options
- High-Temperature Epoxy Bonding
Product Description
HumiSeal® UV23 is a single-component, epoxy-based UV-curable adhesive and encapsulant designed for electronic applications requiring UV-initiated curing, chemical resistance, and high-temperature performance. The clear formulation has a viscosity of 9,500–14,500 cP at 25°C and requires direct UV exposure. For optimal physical and chemical properties, a two-stage curing process is recommended, consisting of UV exposure followed by 16 hours of room-temperature curing or 1 hour of thermal curing at 135°C. The cured epoxy exhibits Shore D75 hardness and an operating temperature range of -50°C to 150°C. An ultimate glass transition temperature (Tg) of 135°C can be achieved through the recommended thermal post-cure. HumiSeal UV23 is suitable for applications involving metals, ceramics, and glass and is REACH and RoHS compliant.
Key features
- UV-initiated curing: UV-gellable epoxy requiring direct UV exposure, with mercury (H) or iron (D) doped bulbs suitable for initiating the curing process
- High-temperature performance: Operating temperature range of -50°C to 150°C, with an ultimate glass transition temperature of 135°C.
- Chemical resistance: Epoxy formulation designed to provide chemical resistance, with optimal properties achieved through recommended post-curing.
Applications
Electronic adhesive bonding, encapsulation, and sealing applications involving metals, ceramics, and glass.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Mechanical Properties
Additional Information
Cure Parameters for HumiSeal® UV23
HumiSeal® UV23 should be cured for best properties by a two-stage process including UV exposure and room/thermal post-cure.
Storage
HumiSeal® UV23 should be stored between 8°C and 28°C in tightly closed containers away from direct sunlight and light sources. Shelf life is six months from DOM.
Caution
Application of HumiSeal® UV23 should be carried out in accordance with local and national health and safety regulations. Use only in well-ventilated areas to avoid inhalation of vapor. Avoid contact with skin and eyes. Consult SDS prior to use.