EPOCAP 43648
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- 10,000 cP Part A Viscosity
- 100:14 43648/55137 Weight Mix
- Composite and Electrical Potting Use
Product Description
EPOCAP 43648 Part A is the resin component of the EPOCAP 43648-55137 low-viscosity, two-component epoxy adhesive and laminating system. Part A is a clear amber liquid with typical viscosity of 10,000 cP and specific gravity of 1.16 at 25 deg C. In the paired system, 43648 Part A mixes with 55137 Part B at 100:14 by weight or 8.45:1 by volume. The paired system is used for reinforced-composite assembly, composite fabrication, laminating, and electrical potting. Cured-system values apply only to the 43648/55137 pairing and do not describe Part A alone.
Key features
- Part A Viscosity: Typical viscosity is 10,000 cP at 25 deg C, with specific gravity of 1.16 for the clear amber resin.
- 43648/55137 Mix Ratio: The paired system uses 100:14 by weight or 8.45:1 by volume.
- Composite and Electrical Potting Use: The 43648/55137 system is used for composite assembly, fabrication, laminating, and electrical potting.
Applications
Resin component for the 43648-55137 composite assembly, laminating, and electrical-potting system.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Legacy-source typical values for EPOCAP 43648 Part A only.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Clear amber | - | Legacy source; Part A; as supplied |
| Viscosity | 10,000 | cP | Legacy source; Part A; 25 deg C |
| Weight per gallon | 9.67 | lb/gal | Legacy source; Part A |
| Specific gravity | 1.16 | - | Legacy source; Part A; 25 deg C |
| Shelf life | 12 | months | Legacy source; Part A in a separate sealed container |